Stainless steel

Welded stainless steel | Seamless stainless steel
Stainless Steel

Welded and calibrated Stainless steel heat exchanger tubes, V= 1.0

Certification to EN 10204 / 3.1 - 3.2
ISO9001 - PED 97/23/EC


Third party inspection by:

  • Lloyd’s Reg.of Shipping
  • TÜV
  • DNV
  • GL
  • or to other requirements


Specification to:AD-2000 W2



Grades
EN Tolerances: Testing:

1.4301
1.4307
1.4401
1.4404
1.4435
1.4541
1.4571

1.4462
1.4539

EN 10217-7 / TC 1/2
EN 10217-7 / TC 1/2
EN 10217-7 / TC 1/2
EN 10217-7 / TC 1/2
EN 10217-7 / TC 1/2
EN 10217-7 / TC 1/2
EN 10217-7 / TC 1/2

SEW 400
SEW 400

DIN 28181 TK I
EN 1127 D3T3
EN 1127 D4T3
EN 1127 D4T4

D3: ± 0,75%, Min ± 0,30 mm
D4: ± 0,50%, Min ± 0,10 mm
T3: ± 10%, Min ± 0,2 mm
T4: ± 7,5%, Min ± 0,15 mm

or to other
requirements

100% Eddy current
or
Hydrostatic testing

Intergranular
corrosion
DIN-EN-ISO 3651-2

P.M.I.

or to other
requirements

Grades
ASTM / ASME Tolerances Testing:

TP 304
TP 304L
TP 316
TP 316L
TP 321
TP 904 L
S 31803

A / SA 249 - A / SA 269
A / SA 249 - A / SA 269
A / SA 249 - A / SA 269
A / SA 249 - A / SA 269
A / SA 249 - A / SA 269
B 374
A / SA 789

A/1016 / A1016M
A / SA 450




100% Eddy current
or
Hydrostatic testing

Intergranular
corrosion
A262 Practice E

P.M.I.

or to other
requirements

Wallthickness: Min. Wall -0/+20%, Av. Wall +/-10%

seamless

Welded stainless steel | Seamless stainless steel
Stainless Steel

Seamless cold finished stainless steel heat exchanger tubes

Certification to EN 10204 / 3.1 - 3.2
ISO9001 - PED 97/23/EC


Third party inspection by:

  • Lloyd’s Reg.of Shipping
  • TÜV
  • DNV
  • GL
  • or to other requirements


Specification to:AD-2000 W2

Grades
EN Tolerances: Testing:

1.4301
1.4306
1.4541
1.4571
1.4401
1.4404
1.4435
1.4439

1.4462
1.4539

EN 10216-5 / TC1/2
EN 10216-5 / TC1/2
EN 10216-5 / TC1/2
EN 10216-5 / TC1/2
EN 10216-5 / TC1/2
EN 10216-5 / TC1/2
EN 10216-5 / TC1/2
EN 10216-5 / TC1/2

SEW 400
SEW 400

DIN 28180 TK I
EN 1127 D3T3
EN 1127 D4T3
EN 1127 D4T4

D3: ± 0,75%, Min ± 0,30 mm
D4: ± 0,50%, Min ± 0,10 mm
T3: ± 10%, Min ± 0,2 mm
T4: ± 7,5%, Min ± 0,15 mm


or to other requirements


100% Eddy current
or
Hydrostatic testing

Intergranular
corrosion
DIN-EN-ISO 3651-2

P.M.I.

or to other
requirements
Grades to: ASTM / ASME Tolerances: Testing:

TP 304
TP 304 L/H
TP 321
TP 321H
TP 316 Ti
TP 316
TP 316 L/H
TP 904 L

S 31803
S 32750
S 32760

TP 405
TP 410
TP 430

A / SA 213 - A / SA 269
A / SA 213 - A / SA 269

A / SA 213 - A / SA 269
A / SA 213 - A / SA 269
A / SA 213 - A / SA 269
A / SA 213 - A / SA 269
A / SA 213 - A / SA 269

A / SA 269

A / SA 789
A / SA 789
A / SA 789

A / SA 268
A / SA 268
A / SA 268

A/1016 / A1016M
A/SA 450



100% Eddy current
or
Hydrostatic testing

Intergranular
corrosion
A262 Practice E

P.M.I.

or to other
requirements

Wallthickness: Min. Wall -0/+20%, Av. Wall +/-10%